Titanium 6-2-4-6 is a heat treatable alpha-beta alloy, with which you can achieve higher strengths than with Titanium 6/4. The advantages of Titanium 6-2-4-6 are an increased strength, low cycle fatig
Titanium 6-2-4-6 is a heat treatable alpha-beta alloy, with which you can achieve higher strengths than with Titanium 6/4. The advantages of Titanium 6-2-4-6 are an increased strength, low cycle fatigue and its ductility. It has a high strength at temperatures up to 450 ° C.
Advantages of Titanium 6Al/2Sn/4Zr/6Mo
Low modulus of Elasticity
Low Density to Weight Ratio
Resistance to Fatigue
Heat Treatable to attain higher strengths
Material Data Sheet
| Alloy | Titan 6AL-2Sn-4Zr-6Mo |
| UNS | UNS R56260 |
| Norm | Titanium 6-2-4-6 |
Main fields of application of alloy Ti-Gr-6-2-4-6
Typical applications are in the intermediate stage compressors turbines, discs, blades and sour gas applications as well as in oil and gas industry.
Chemical composition of alloy Ti-Gr-6-2-4-6
| Al | ≤ % 5.5 < 6.5 | C | ≤ % 0.04 max |
| Su | ≤ % 1.75 < 2.25 | N | ≤ % 0.04 max |
| Zr | ≤ % 3.6 <4.4 | H | ≤ % 0.125 max |
| Mo | ≤ % 5.5 <6.5 | Cu | ≤ % 0.50 |
| Fe | ≤ % 0.015 max | Fe | ≤ % 1.5 |
| O | ≤ % 0.15 max | Res | ≤ % 0.30 |
Properties
| Melting Range | 1595- 1675°C |
| Density | 4.64 g/cm³ |
| Modulus | 20° C 70-114 GPa |
| Beta Transus | 935°C |
Fatigue Failure and good resistance to fatigue
Specifications
The Hempel stock typically meets the following requirements:
MIL-T-9047
AMS 2631 Class A
The material is delivered with 3.1 certification.
3.2 Certification is available at extra cost.
Filler metal
not available
Delivery program
The Hempel Special Metal delivery program for Titanium 6-2-4-6 contains:
Sheets and plates 1.6 mm - 40 mm
Bars dia. 12 mm - 150 mm